Oxide

Origin: The basic material for the preparation of reference specimens originates primarily from our own production.

Specimen preparation comprises the preparation of the analytical-fineness specimen material, careful homogenisation, homogeneity testing and determination of particle-size distribution.

Certification is accomplished by means of expression in SI units (mol, kg), and is based on the reconstitution procedure, using high-purity substances with defined impurity contents.

Storage in small quantities, with the exclusion of air or under an inert gas. Stability checks are performed at regular intervals.

Packing unit: Quantities of 100 g (for macrosynthetic specimens: 20 g) in high-quality glass containers.

certified reference material Ca-aluminate (Code: SX01)

Analyte Content in SX01-01 SX01-02 SX01-03
CaO % 26.74 18.34 23.38
SiO2 % 0.17 2.02 0.450
Fe2O3 % 0.118 0.708 0.289
MnO % 0.008 0.114 0.024
S % 0.011 0.020 -.-
Al2O3 % 72.2 64.30 68.8
MgO % 0.191 12.54 3.53
TiO2 % -.- 0.165 0.067
K2O % -.- -.- 0.296
SrO % -.- 0.024 0.009
V2O5 % < 0.005 1.48 2.36
Cr2O3 % 0.006 0.054 0.028
MoO3 % -.- -.- 0.014
Dimension < 0.125 mm < 0.125 mm < 0.125 mm

certified reference material Cement (Code: SX02)

Analyte Content in SX02-09 SX02-11 SX02-12
Ca % 48.78 40.63 46.48
SiO2 % 21.95 25.04 21.16
Fe2O3 % 0.204 2.98 3.94
Mn3O4 % 0.025 0.172 0.062
P2O5 % 0.043 0.137 0.191
S % 1.19 1.48 1.18
Al2O3 % 4.63 6.86 4.41
MgO % 0.717 2.79 0.945
TiO2 % 0.095 0.319 0.242
Na2O % 0.078 0.156 0.084
K2O % 1.01 0.524 0.495
Be % 0.4 3.1 1.3
SrO % 0.051 0.083 0.086
BaO % 0.028 0.041 0.0223
La % 11.1 47 58
Zr % 0.00255 0.0133 0.0110
V % 18.0 77 103
Cr % 0.00153 0.0032 0.0074
Mo % < 2.0 2.0 2.2
Co % < 0.8 7.6 10.1
Ni % 7.5 20.7 30
Cu % 12.2 65 52
Zn % 13.0 402 497
Cd % < 0.4 < 0.4 < 0.4
In % < 0.3 < 0.4 < 0.2
Tl % < 0.6 < 0.6 < 0.7
Pb % 50.8 29.3 24.9
As % < 0.6 26.9 48
Sb % < 0.5 1.6 2.2
Bi % < 0.3 < 0.3 < 0.5
Se % < 2.4 1.6 < 2.9
Te % < 0.8 < 1.4 < 0.8
Ce % 12.7 65 52
Th % 2.4 8.3 6.3
U % 0.8 5.7 2.8
Dimension < 0.100 mm < 0.100 mm < 0.100 mm

certified reference material Dolomite subst. (Code: SX07)

Analyte Content in SX07-11 SX07-12
CaO % 32.46 20.16
SiO2 % 12.07 13.30
Fe % 8.81 6.72
Mn3O4 % 1.745 0.906
P2O5 % 0.262 0.141
S % 0.314 0.129
Al2O3 % 9.49 20.79
MgO % 28.57 32.62
TiO2 % 0.370 0.671
Na2O % -.- 0.167
K2O % 0.092 0.146
SrO % 0.029 0.016
ZrO2 % 0.068 0.383
V2O5 % 0.056 0.039
Nb2O5 % -.- 0.012
Cr2O3 % 0.84 0.560
NiO % 0.020 0.050
ZnO % 0.183 0.052
PbO % 0.015 0.008
Dimension < 0.125 mm < 0.125 mm

certified reference material Dolomite stone (Code: SX09)

Analyte Content in SX09-15
CaO % 30.59
SiO2 % 0.035
Fe2O3 % 0.191
MnO % 0.050
P2O5 % 0.008
Al2O3 % 0.019
MgO % 21.21
Na2O % 0.026
K2O % 0.007
Dimension < 0.125 mm

certified reference material Iron ore (Code: SX11)

Analyte Content in SX11-15 SX11-16 SX11-18 SX11-35 SX11-37
CaO % 0.494 1.149 0.052 0.011 1.930
SiO2 % 5.79 4.67 1.56 0.696 2.365
Fe % 63.17 64.69 64.72 64.69 66.15
FeO % -.- -.- -.- 0.06 0.32
Mn % 0.074 0.198 0.713 1.520 0.038
P2O5 % 0.101 0.058 0.141 0.140 0.113
S % -.- -.- 0.009 0.006 0.003
Al2O3 % 2.68 0.722 1.785 1.49 0.442
MgO % 0.244 0.400 0.057 0.033 0.164
TiO2 % 0.128 0.078 0.075 0.052 0.032
Na2O % 0.020 0.016 0.014 -.- 0.020
K2O % 0.008 0.023 0.020 0.016 0.011
V2O5 % 0.010 0.009 0.017 -.- -.-
Cr2O3 % 0.005 0.038 -.- -.- 0.017
NiO % -.- 0.011 -.- -.- -.-
ZnO % -.- 0.0010 0.005 -.- -.-
CO2 % -.- 0.026 0.033 0.007 0.089
C tot. % -.- 0.016 0.085 0.069 0.101
H2O 900°C % -.- 0.059 2.51 2.31 0.080
Dimension < 0.100 mm < 0.100 mm < 0.100 mm < 0.100 mm < 0.100 mm

certified reference material Feldspar (Code: SX16)

Analyte Content in SX16-02
CaO % 0.032
SiO2 % 66.93
Fe % 0.047
MnO % 0.001
P2O5 % 0.087
Al2O3 % 17.16
TiO2 % 0.038
K2O % 14.19
SrO % 0.036
BaO % 0.323
PbO % 0.012
Dimension < 0.125 mm

certified reference material Nb-ore concentr. (Code: SX18)

Analyte Content in SX18-03 SX18-06
CaO % 13.02 27.77
SiO2 % 1.91 3.38
Fe % 3.50 5.44
MnO % 0.325 1.12
P2O5 % 0.102 1.75
S % 0.051 0.798
Al2O3 % 0.291 0.945
MgO % 0.136 16.16
TiO2 % 4.26 0.078
Na2O % 5.28 0.061
K2O % 0.233 0.525
SrO % 1.20 0.274
BaO % 0.201 0.0445
Y2O3 % 0.085 0.0090
La2O3 % 0.153 0.0420
ZrO2 % 0.847 0.0278
V2O5 % 0.073 0.0096
Nb2O5 % 60.62 0.098
Ta2O5 % 0.273 < 0.001
ZnO % < 0.003 0.0137
SnO2 % -.- < 0.0001
CeO2 % 0.556 0.083
Nd2O3 % 0.207 0.0387
ThO2 % 0.770 0.0089
U3O8 % 0.202 0.0017
F % 3.65 -.-
CO2 % 0.097 36.82
H2O 900°C % 0.664 0.65
Dimension < 0.125 mm < 0.125 mm

certified reference material Refractory (Code: SX26)

Analyte Content in SX26-12 SX26-15
CaO % 1.80 0.261
SiO2 % 40.80 52.69
Fe2O3 % 3.10 1.613
Mn3O4 % 0.135 0.011
P2O5 % 0.279 0.092
Al2O3 % 36.45 42.17
MgO % 13.13 0.295
TiO2 % 1.25 1.387
Na2O % 0.242 0.115
K2O % 0.759 0.778
SrO % -.- 0.019
BaO % -.- 0.029
ZrO2 % 0.163 0.108
V2O5 % 0.027 0.027
Cr2O3 % 0.385 0.099
WO3 % -.- 0.060
NiO % 0.032 -.-
C tot. % 0.437 0.023
CO2 % 0.54 -.-
H2O 900°C % 0.75 -.-
Dimension < 0.125 mm < 0,125 mm

certified reference material Fluorspar (Code: SX27)

Analyte Content in SX27-09
Ca % 39.98
SiO2 % 3.93
Fe2O3 % 15.72
MnO % 0.077
SO4 % 0.027
Al2O3 % 0.310
MgO % 0.017
Na2O % 0.030
K2O % 0.029
Cr2O3 % 0.004
CuO % 0.052
ZnO % 0.004
F % 38.10
CO2 % 0.027
H2O 900°C % 0.929
Dimension < 0.125 mm

certified reference material Cont.cast.powder (Code: SX28)

Analyte Content in SX28-01 SX28-02
Ca % 23.08 25.15
SiO2 % 55.0 57.50
Fe2O3 % 0.467 0.488
MnO % 0.033 0.030
P2O5 % 0.044 0.060
S % 0.245 0.132
Al2O3 % 3.58 3.09
MgO % 4.80 0.981
TiO2 % 0.069 0.055
Na2O % 1.33 1.097
K2O % 1.092 0.830
SrO % 0.019 0.020
BaO % 0.019 -.-
ZnO % -.- 0.004
F % 0.047 0.074
Dimension < 0.125 mm < 0.125 mm

certified reference material BF flue dust (Code: SX29)

Analyte Content in SX29-01 SX29-02 SX29-03
CaO % 5.28 3.12 2.00
SiO2 % 4.28 3.28 2.44
Fe % 59.37 61.67 63.01
Mn % 0.367 0.341 0.425
P2O5 % 0.153 0.165 0.158
S % 0.488 0.577 0.392
SO3 % -.- 1.44 -.-
Al2O3 % 0.961 0.823 0.701
MgO % 1.147 0.678 0.502
TiO2 % 0.068 0.053 0.058
Na2O % 0.119 0.138 0.111
K2O % 0.778 0.84 0.705
V2O5 % 0.020 -.- 0.020
Cr2O3 % 0.038 0.037 0.040
NiO % 0.015 0.016 0.012
CuO % -.- -.- 0.006
ZnO % 0.267 0.271 1.19
PbO % 0.006 0.017 0.018
Dimension <0.125 mm <0.125 mm < 0.125 mm

certified reference material Casting powder (Code: SX30)

Analyte Content in SX30-14
Ca % 25.84
SiO2 % 30.83
Fe2O3 % 1.25
Mn3O4 % 0.065
P2O5 % 0.108
S % 0.080
Al2O3 % 4.87
MgO % 1.737
TiO2 % 0.208
Na2O % 4.38
K2O % 0.181
SrO % 0.053
V2O5 % 0.036
NiO % 0.067
F % 6.60
C tot. % 8.11
Dimension < 0,125 mm

certified reference material BF-slag (Code: SX32)

Analyte Content in SX32-26 SX32-28 SX32-32 SX32-33 SX32-34 SX32-35 SX32-39
CaO % 41.95 35.66 36.59 36.30 37.22 34.35 42.96
Ca % -.- -.- -.- -.- -.- 24.55 -.-
SiO2 % 35.92 38.69 39.03 41.53 41.28 39.33 36.54
Fe % 0.174 0.332 0.417 1.72 0.742 2.87 0.188
Mn % 0.236 1.342 0.671 0.907 0.970 0.341 0.158
P2O5 % 0.005 0.014 -.- 0.026 -.- 0.015 -.-
S % 1.17 0.812 1.06 0.804 0.88 1.539 1.065
Al2O3 % 13.01 11.93 11.81 11.53 11.27 15.68 10.85
MgO % 6.37 8.56 8.12 5.27 5.37 6.289 7.02
TiO2 % 0.614 0.638 0.589 0.621 0.618 0.229 0.435
Na2O % 0.265 0.388 0.437 0.193 0.322 0.103 0.232
K2O % 0.407 1.235 1.228 0.462 0.890 0.090 0.332
SrO % 0.064 0.062 0.076 0.047 0.048 0.072 0.069
BaO % 0.093 0.097 0.087 0.082 0.087 0.107 0.069
Y % -.- -.- -.- -.- -.- -.- 0.006
ZrO2 % 0.039 0.035 0.022 0.046 0.042 0.064 0.037
V2O5 % -.- 0.007 -.- 0.019 0.016 0.004 -.-
Cr2O3 % -.- -.- -.- 0.021 0.018 0.005 -.-
Dimension < 0.125 mm < 0.125 mm < 0.125 mm < 0.125 mm < 0.125 mm < 0.125 mm < 0.0125 mm

certified reference material Limestone (Code: SX35)

Analyte Content in SX35-13
CaO % 55.06
SiO2 % 0.289
Fe2O3 % 0.082
MnO % 0.017
P2O5 % 0.007
SO3 % 0.012
Al2O3 % 0.097
MgO % 0.466
TiO2 % 0.006
Na2O % 0.003
K2O % 0.029
SrO % 0.019
CO2 % 43.80
H2O 900°C % 0.099
Dimension < 0.125 mm

certified reference material Gravel (Code: SX36)

Analyte Content in SX36-09 SX36-10
CaO % 0.047 0.008
SiO2 % 96.44 98.80
Fe2O3 % 0.703 0.419
Mn3O4 % 0.020 0.009
P2O5 % 0.019 -.-
S % -.- 0.009
Al2O3 % 1.46 0.234
MgO % 0.104 -.-
TiO2 % 0.086 -.-
Na2O % 0.045 < 0.003
K2O % 0.334 0.014
Cr2O3 % 0.029 0.030
Co3O4 % 53 -.-
CO2 % 0.010 -.-
H2O 900°C % 0.48 0.153
Dimension < 0.125 mm < 0.125 mm

certified reference material Coke ash (Code: SX37)

Analyte Content in SX37-13
CaO % 4.16
SiO2 % 49.74
Fe2O3 % 8.57
MnO % 0.172
P2O5 % 0.215
S % 0.228
Al2O3 % 26.33
MgO % 2.94
TiO2 % 1.095
Na2O % 0.568
K2O % 4.120
SrO % 0.056
BaO % 0.170
ZrO2 % 0.028
V2O5 % 0.060
Cr2O3 % 0.046
Co3O4 % 0.011
NiO % 0.026
CuO % 0.037
ZnO % 0.232
PbO % 0.209
Dimension < 0.100 mm

certified reference material LD-slag (Code: SX39)

Analyte Content in SX39-08 SX39-27 SX39-31
CaO % 47.10 37.27 40.40
SiO2 % 12.40 12.58 12.92
Fe % 18.95 23.35 19.45
Mn % 4.31 2.498 3.39
P2O5 % 1.488 0.798 1.195
S % 0.114 0.232 0.083
Al2O3 % 1.097 3.39 3.38
MgO % 2.511 5.83 8.12
TiO2 % 0.558 0.424 0.432
K2O % 0.008 0.109 0.006
SrO % 0.028 0.032 0.022
V2O5 % 0.273 0.157 0.192
Nb2O5 % 0.072 0.043 0.068
Cr % 0.339 0.830 0.201
Mo % -.- 0.0074 -.-
MoO3 % -.- -.- 0.028
Co % -.- 0.0007 -.-
Ni % -.- 0.0042 -.-
Cu % -.- 0.0017 -.-
Zn % -.- 0.0054 -.-
Cd % -.- < 0.0001 -.-
B % -.- 0.0036 -.-
Tl % -.- < 0.0000 -.-
Pb % -.- 0.0009 -.-
As % -.- < 0.0004 -.-
Se % -.- < 0.0003 -.-
Dimension < 0.125 mm <0.125 mm <0,125 mm

certified reference material Mg-stone (Code: SX42)

Analyte Content in SX42-08
CaO % 2.06
SiO2 % 5.09
Fe2O3 % 1.49
Mn3O4 % 0.070
P2O5 % 0.077
SO3 % 0.018
Al2O3 % 41.66
MgO % 47.83
TiO2 % 0.066
K2O % 0.037
ZrO2 % 0.091
Cr2O3 % < 0.080
ZnO % 0.006
CO2 % 0.58
C tot. % 0.353
H2O 900°C % 0.89
Dimension < 0.125 mm

certified reference material Slide sand (Code: SX45)

Analyte Content in SX45-01 SX45-02 SX45-06 SX45-07
CaO % 0.025 0.038 -.- 0.096
SiO2 % 72.21 65.97 10.22 27.95
Fe tot. % 5.14 6.31 17.51 14.51
Mn3O4 % 0.065 0.074 0.703 0.179
P2O5 % -.- 0.007 -.- -.-
S % -.- -.- 0.007 -.-
Al2O3 % 4.92 5.69 12.93 11.00
MgO % 2.40 3.24 8.18 7.29
TiO2 % 0.195 0.203 0.510 0.486
Na2O % 0.059 0.062 -.- -.-
K2O % 0.633 0.693 -.- -.-
V2O5 % 0.102 0.110 0.382 0.270
Cr2O3 % 11.53 14.75 42.01 33.41
WO3 % -.- -.- -.- 0.019
NiO % 0.053 0.033 -.- 0.090
C tot. % 0.607 0.471 0.700 0.326
CO2 % -.- -.- -.- 0.013
H2O 900°C % 0.204 0.177 0.091 0.129
Dimension < 0.080 mm < 0.080 mm < 0.125 mm < 0.125 mm

certified reference material Mo-oxid (Code: SX47)

Analyte Content in SX47-06 SX47-07
CaO % 0.644 1.61
SiO2 % 7.52 4.38
Fe2O3 % 3.83 1.80
MnO % 0.036 0.008
S % 0.050 0.069
Al2O3 % 1.178 0.702
MgO % 0.207 0.117
TiO2 % 0.092 0.040
Na2O % 1.009 0.045
K2O % 0.407 0.182
Cr2O3 % -.- 0.004
Mo % 57.55 61.08
CuO % 0.106 0.504
ZnO % -.- 0.064
C tot. % 0.016 0.040
Dimension < 0.125 mm < 0.125 mm

certified reference material Olivine (Code: SX49)

Analyte Content in SX49-12
CaO % 0.081
SiO2 % 41.6
Fe tot. % 5.07
MnO % 0.096
Al2O3 % 0.432
MgO % 49.18
TiO2 % 0.002
K2O % 0.014
Cr2O3 % 0.383
Co3O4 % 0.016
NiO % 0.354
C tot. % 0.054
CO2 % 0.046
H2O 900°C % 1.25
Dimension < 0.125 mm

certified reference material Vacuum slag (Code: SX51)

Analyte Content in SX51-09 SX51-20 SX51-21
CaO % 53.00 52.90 51.14
SiO2 % 8.92 8.13 7.63
Fe % 1.36 1.55 1.27
Mn % 1.46 1.27 0.769
P2O5 % 0.036 0.039 0.028
S % 0.341 0.281 0.369
Al2O3 % 20.27 20.33 23.56
MgO % 11.02 11.68 11.98
TiO2 % 1.361 1.28 0.869
K2O % 0.010 0.011 0.011
SrO % 0.035 0.032 0.031
ZrO2 % 0.013 0.230 0.232
V2O5 % 0.015 0.016 0.012
Nb2O5 % 0.122 0.202 0.109
Cr % 0.053 -.- 0.039
Cr2O3 % -.- 0.039 -.-
Mo % 0.0012 -.- -.-
Co % < 0.0003 -.- -.-
Ni % 0.0018 -.- -.-
Cu % 0.0010 -.- -.-
Zn % < 0.0006 -.- -.-
Cd % 0.00005 -.- -.-
B % 0.0104 -.- -.-
Tl % < 0.0001 -.- -.-
Pb % 0.0001 -.- -.-
As % < 0.0001 -.- -.-
Se % 0.0093 -.- -.-
Dimension < 0.125 mm < 0.125 mm < 0.125 mm

certified reference material Iron ore sinter (Code: SX56)

Analyte Content in SX56-16 SX56-30 SX56-31 SX56-32 SX56-35
CaO % 9.51 6.99 6.28 10.79 6.11
SiO2 % 5.18 3.98 5.08 5.55 4.81
Fe % 57.29 -.- -.- -.- 59.22
FeO % 6.58 4.86 5.41 4.06 5.27
Fe tot. % -.- 60.62 58.54 55.03 -.-
Mn % 0.477 0.298 0.945 0.708 0.368
P2O5 % 0.140 0.112 0.107 0.104 0.120
S % -.- 0.011 0.007 0.061 0.013
Al2O3 % 1.331 1.134 1.42 1.281 1.392
MgO % 1.491 0.654 2.01 2.070 0.882
TiO2 % 0.101 0.085 0.076 0.068 0.224
Na2O % 0.025 0.032 0.046 0.048 0.047
K2O % 0.045 0.040 0.247 0.174 0.066
V2O5 % 0.018 -.- 0.005 -.- -.-
Cr2O3 % 0.045 -.- 0.015 -.- 0.031
NiO % -.- -.- 0.005 -.- -.-
ZnO % 0.013 0.016 0.040 0.026 0.010
H2O 900°C % -.- -.- -.- -.- 1.27
Dimension < 0.063 mm < 0.063 mm < 0.063 mm < 0.063 mm <0.063 mm

certified reference material Cover.powder (a) (Code: SX57)

Analyte Content in SX57-04 SX57-05 SX57-06 SX57-07 SX57-08
CaO % 0.302 2.51 1.04 1.78 0.966
SiO2 % 92.49 76.31 87.92 82.15 86.72
Fe2O3 % 0.090 2.89 0.125 1.50 0.931
Mn3O4 % 0.067 0.263 0.291 0.278 0.126
P2O5 % 0.273 0.123 0.755 0.443 0.226
S % 0.071 0.164 0.242 0.210 0.102
Al2O3 % 0.198 0.363 0.073 0.223 1.15
MgO % 0.362 9.60 0.526 5.086 3.10
TiO2 % -.- 0.217 0.231 0.223 0.126
Na2O % 0.070 0.116 0.124 0.117 0.085
K2O % 0.97 0.653 3.10 1.89 0.872
C tot. % 3.60 4.33 3.62 4.03 3.83
CO2 % 0.008 0.265 0.056 0.158 0.094
H2O 900°C % 1.38 2.32 1.38 1.82 1.70
Dimension < 0.125 mm < 0.125 mm < 0.125 mm < 0.125 mm < 0.125 mm

certified reference material Cover.powder (b) (Code: SX59)

Analyte Content in SX59-05 SX59-06
CaO % 46.51 33.29
SiO2 % 22.89 30.78
Fe2O3 % 0.441 0.598
Mn3O4 % < 0.062 0.052
P2O5 % 0.039 0.037
S % 0.074 0.061
Al2O3 % 19.35 14.34
MgO % 9.24 19.38
TiO2 % 0.037 0.037
Na2O % 0.443 0.32
K2O % 0.322 0.210
SrO % -.- 0.015
Dimension < 0.125 mm < 0.125 mm

certified reference material Cupola dust (Code: SX62)

Analyte Content in SX62-06
CaO % 0.090
SiO2 % 0.430
Fe2O3 % 0.572
Mn3O4 % 0.061
Mn % 0.04
P2O5 % 0.191
S % 0.305
Al2O3 % 0.220
MgO % 0.020
TiO2 % 0.014
Na2O % 0.085
K2O % 0.086
Cr2O3 % 0.048
Ni % 2968
Cu % 2.021
ZnO % 91.1
SnO2 % 0.047
F % 0.071
C tot. % 2.57
H2O 900°C % 1.17
Dimension < 0.100 mm

certified reference material Tundish g. Mat. (Code: SX66)

Analyte Content in SX66-04 SX66-05 SX66-06
CaO % 1.609 1.35 1.377
SiO2 % 24.75 27.08 27.49
Fe2O3 % 4.62 4.94 4.91
Mn3O4 % 0.098 -.- 0.097
MnO % -.- 0.105 -.-
P2O5 % 0.084 0.041 0.057
SO3 % 0.026 -.- 0.052
S % -.- 0.019 -.-
Al2O3 % 1.884 1.252 1.301
MgO % 64.45 62.58 62.70
TiO2 % 0.141 0.090 0.101
Na2O % 0.516 0.347 -.-
K2O % 0.089 0.072 0.069
Cr2O3 % 0.255 0.223 0.216
Co3O4 % -.- 0.010 -.-
NiO % 0.165 0.220 0.216
CO2 % 0.35 -.- -.-
C tot. % 0.471 0.38 0.38
H2O 900°C % 1.02 -.- 1.15
Dimension < 0.125 mm < 0.125 mm < 0.125 mm

certified reference material Ilmenite (Code: SX67)

Analyte Content in SX67-06
CaO % 1.179
SiO2 % 7.31
Fe tot. % 36.83
Mn % 0.094
P2O5 % 0.017
S % 0.288
Al2O3 % 4.46
MgO % 2.82
TiO2 % 32.37
K2O % 0.118
SrO % 0.016
ZrO2 % 0.044
V2O5 % 0.285
Cr2O3 % 0.143
Co3O4 % 0.024
NiO % 0.049
CuO % 0.017
ZnO % 0.020
C tot. % 0.044
Dimension < 0.100 mm

certified reference material Mn-slag (Code: SX74)

Analyte Content in SX74-03 SX74-04
CaO % 15.95 26.16
SiO2 % 43.23 37.39
Fe % 0.088 0.086
Mn % 4.93 2.66
S % 0.818 0.959
Al2O3 % 19.84 24.61
MgO % 12.34 7.04
TiO2 % 0.100 0.164
Na2O % 0.433 -.-
K2O % 1.30 0.630
SrO % 0.083 0.109
Ba % -.- 0.925
Y2O3 % -.- 0.014
ZrO2 % 0.039 0.035
Cr2O3 % 0.007 0.007
CO2 % 0.032 -.-
H2O 900°C % 0.062 -.-
Dimension < 0.125 mm < 0.125 mm