Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
CaO |
% |
0.090 |
0.002 |
3 |
1 |
P2O5 |
% |
0.191 |
0.002 |
3 |
1 |
Na2O |
% |
0.085 |
0.001 |
3 |
2 |
ZnO |
% |
91.1 |
0.2 |
3 |
1 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
2: Atomic absorption spectrometry |
3: Specific ion electrode end point |
4: Combustion with IR-detection |
5: detection with IR-/ UV-absorption after Combustion |
  |
Comment |
Thermal treatment of material before weighing: 105°C, 4 h |