SX57-05
Uncover compound

Version: 003      Date of certification: 25.06.08      Sample form: Powder < 0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe2O3
Mn3O4
P2O5
  %
%
%
%
%
      2.51
76.31
2.89
0.263
0.123
      0.02
0.14
0.02
0.002
0.003
 3
3
3
3
3
1
1
1
1
1
  S
Al2O3
MgO
TiO2
Na2O
  %
%
%
%
%
      0.164
0.363
9.60
0.217
0.116
      0.006
0.011
0.05
0.004
0.005
 3
3
3
3
3
2
1
1
1
3
  K2O
C tot.
CO2
H2O 900°C
  %
%
%
%
      0.653
4.33
0.265
2.32
      0.006
0.03
0.011
0.03
 3
3
3
3
1
2
4
5
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection
3: Atomic absorption spectrometry
4: Digestion by acids, coulometric detection
5: detection with IR-/ UV-absorption after combustion
 

Comment
Thermal treatment of material before weighing: 105°C, 1 h