CERTIFIED REFERENCE MATERIAL
SX57-08
Uncover compound

Version: 001      Date of certification: 27.05.08      Sample form: Powder < 0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe2O3
Mn3O4
P2O5
  %
%
%
%
%
      0.966
86.72
0.931
0.126
0.226
      0.007
0.15
0.012
0.001
0.005
 3
4
3
3
3
1
1
1
1
1
  S
Al2O3
MgO
TiO2
Na2O
  %
%
%
%
%
      0.102
1.15
3.10
0.126
0.085
      0.004
0.01
0.02
0.002
0.001
 3
3
3
3
3
2
1
1
1
3
  K2O
C tot.
CO2
H2O 900°C
  %
%
%
%
      0.872
3.83
0.094
1.70
      0.009
0.02
0.009
0.04
 3
3
3
3
1
2
4
5
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection
3: Atomic absorption spectrometry
4: Digestion by acids, coulometric detection
5: detection with IR-/ UV-absorption after combustion