Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
Ca |
% |
39.98 |
0.10 |
5 |
1 |
Al2O3 |
% |
0.310 |
0.005 |
5 |
1 |
CuO |
% |
0.052 |
0.001 |
5 |
1 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
2: Atomic absorption spectrometry |
3: Digestion by acids, coulometric detection |
4: Heat conductivity after reduction |
Comment |
Thermal treatment of material before weighing: 105°C, 4 h |