Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX01-01
Ca-aluminate

Version: 003      Date of certification: 01.07.10      Sample form: Powder < 0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe2O3
MnO
S
  %
%
%
%
%
     26.74
0.17
0.118
0.008
0.011
      0.04
0.01
0.003
0.001
0.001
 8
10
10
7
10
1
1
1
1
1,2
  Al2O3
MgO
V2O5
Cr2O3
  %
%
%
%
     72.2
0.191
< 0.005
0.006
      0.2
0.005
-.-
0.001
 5
8
6
4
1
1
1
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection

Comment
Thermal treatment of material before weighing: 900°C, 1 h