Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
CaO |
% |
1.04 |
0.01 |
3 |
1 |
S |
% |
0.242 |
0.012 |
3 |
2 |
K2O |
% |
3.10 |
0.01 |
3 |
1 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
2: Combustion with IR-detection |
3: Atomic absorption spectrometry |
4: Digestion by acids, coulometric detection |
5: detection with IR-/ UV-absorption after combustion |
  |