Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
CaO |
% |
33.29 |
0.06 |
3 |
1 |
S |
% |
0.061 |
0.002 |
3 |
1 |
K2O |
% |
0.210 |
0.002 |
3 |
1 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
2: Atomic absorption spectrometry |
Comment |
Thermal treatment of material before weighing: 900°C, 1 h |