Laboratory
"Excellence Laboratory Technische Compliance Level III" by GAZ GmbH (Attestation no. GAZ-TCL-12-02-14-01)

CERTIFIED REFERENCE MATERIAL
SX07-12
Dolomite subst.

Version: 002      Date of certification: 25.09.19      Sample form: Powder < 0.125 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe
Mn3O4
P2O5
  %
%
%
%
%
     20.16
13.30
6.72
0.906
0.141
      0.06
0.13
0.02
0.004
0.002
 4
3
5
5
6
1
1
1
1
1
  S
Al2O3
MgO
TiO2
Na2O
  %
%
%
%
%
      0.129
20.79
32.62
0.671
0.167
      0.004
0.14
0.09
0.005
0.001
 8
4
6
6
3
1,2
1
1
1
3
  K2O
SrO
ZrO2
V2O5
Nb2O5
  %
%
%
%
%
      0.146
0.016
0.383
0.039
0.012
      0.002
< 0.001
0.004
0.002
0.001
 6
6
3
6
5
1
1
1
1
1
  Cr2O3
NiO
ZnO
PbO
  %
%
%
%
      0.560
0.050
0.052
0.008
      0.026
0.001
0.003
0.002
 4
6
5
6
1
1
1
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection
3: Atomic absorption spectrometry
 

Comment
Thermal treatment of material before weighing: 900°C, 1 h