Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
CaO |
% |
27.77 |
0.21 |
3 |
1 |
S |
% |
0.798 |
0.022 |
3 |
2 |
K2O |
% |
0.525 |
0.005 |
3 |
1 |
ZrO2 |
% |
0.0278 |
0.0003 |
6 |
1,4 |
SnO2 |
% |
< 0.0001 |
-.- |
3 |
3 |
CO2 |
% |
36.82 |
0.06 |
3 |
7 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
2: Combustion with IR-detection |
3: ICP with quadrupol mass spectrometry |
4: ICP with optical emission spectrometry |
5: ICP with high resolution mass spectrometry |
6: Atomic absorption spectrometry |
7: detection with IR-/ UV-absorption after combustion |
  |
Comment |