Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX29-02
BF casthouse dust

Version: 002      Date of certification: 25.07.06      Sample form: Powder <0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe
Mn
P2O5
  %
%
%
%
%
      3.12
3.28
61.67
0.341
0.165
      0.02
0.03
0.14
0.006
0.005
 3
3
3
3
3
1
1
1
1
1
  S
SO3
Al2O3
MgO
TiO2
  %
%
%
%
%
      0.577
1.44
0.823
0.678
0.053
      0.025
0.06
0.013
0.013
0.001
 3
3
3
3
3
1
1
1
1
1
  Na2O
K2O
Cr2O3
NiO
ZnO
  %
%
%
%
%
      0.138
0.84
0.037
0.016
0.271
      0.002
0.02
0.002
0.002
0.002
 3
3
3
3
3
2
1
1
1
1
  PbO
  %
      0.017
      0.002
 3
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Atomic absorption spectrometry

Comment
Thermal treatment of material before weighing: 600°C, 1 h