Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
CaO | |||||
S | |||||
SrO |
* Measuring method | |
1: X-ray fluorescence spectrometry |   |
Comment |
Thermal treatment of material before weighing: 900°C, 1 h |