"Excellence Laboratory Technische Compliance Level III" by GAZ GmbH (Attestation no. GAZ-TCL-12-02-14-01)

CERTIFIED REFERENCE MATERIAL
SX56-30
Iron ore sinter

Version: 001      Date of certification: 04.09.13      Sample form: Powder < 0.063 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
FeO
Fe tot.
Mn
  %
%
%
%
%
      6.99
3.98
4.86
60.62
0.298
      0.04
0.02
0.05
0.07
0.003
 4
4
4
3
4
1
1
2
1
1
  P2O5
S
Al2O3
MgO
TiO2
  %
%
%
%
%
      0.112
0.011
1.134
0.654
0.085
      0.003
0.001
0.010
0.007
0.001
 4
6
4
4
4
1
3
1
1
1
  Na2O
K2O
ZnO
  %
%
%
      0.032
0.040
0.016
      0.001
0.001
0.001
 3
4
4
4
1
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Titrimetry
3: Combustion with IR-detection
4: Atomic absorption spectrometry

Comment
Thermal treatment of material before weighing: 105°C, 1 h