Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
CaO |
% |
13.02 |
0.03 |
3 |
1 |
S |
% |
0.051 |
0.006 |
3 |
1 |
K2O |
% |
0.233 |
0.009 |
3 |
1 |
ZrO2 |
% |
0.847 |
0.007 |
2 |
1 |
CeO2 |
% |
0.556 |
0.025 |
2 |
1 |
CO2 |
% |
0.097 |
0.003 |
3 |
3 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
2: Atomic absorption spectrometry |
3: detection with IR-/ UV-absorption after combustion |
  |
Comment |
Thermal treatment of material before weighing: 105°C, 4 h |