Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX74-03
Mn-slag

Version: 001      Date of certification: 29.05.08      Sample form: Powder < 0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe
Mn
S
  %
%
%
%
%
     15.95
43.23
0.088
4.93
0.818
      0.03
0.09
0.002
0.01
0.007
 3
3
3
3
3
1
1
1
1
1
  Al2O3
MgO
TiO2
Na2O
K2O
  %
%
%
%
%
     19.84
12.34
0.100
0.433
1.30
      0.03
0.11
0.001
0.007
0.01
 3
3
3
3
3
1
1
1
2
1
  SrO
ZrO2
Cr2O3
CO2
H2O 900°C
  %
%
%
%
%
      0.083
0.039
0.007
0.032
0.062
    < 0.001
0.002
0.001
0.011
0.019
 3
3
3
3
3
1
1
1
3
3
* Measuring method
1: X-ray fluorescence spectrometry
2: Atomic absorption spectrometry
3: detection with IR-/ UV-absorption after combustion