Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX35-13
Limestone

Version: 006      Date of certification: 24.09.10      Sample form: Powder < 0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe2O3
MnO
P2O5
  %
%
%
%
%
     55.06
0.289
0.082
0.017
0.007
      0.17
0.010
0.002
< 0.001
0.001
 3
3
3
3
3
1
1
1
1
1
  SO3
Al2O3
MgO
TiO2
Na2O
  %
%
%
%
%
      0.012
0.097
0.466
0.006
0.003
      0.003
0.005
0.004
< 0.001
0.001
 4
3
3
3
3
1,2
1
1
1
3
  K2O
SrO
CO2
H2O 900°C
  %
%
%
%
      0.029
0.019
43.80
0.099
      0.004
0.001
0.22
0.014
 7
3
3
4
1,3
1
4
5
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection
3: Atomic absorption spectrometry
4: Digestion by acids, coulometric detection
5: detection with IR-/ UV-absorption after Combustion
 

Comment
Thermal treatment of material before weighing: 105°C, 1 h