Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX29-03
BF casthouse dust

Version: 001      Date of certification: 30.01.07      Sample form: Powder < 0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe
Mn
P2O5
  %
%
%
%
%
      2.00
2.44
63.01
0.425
0.158
      0.01
0.02
0.07
0.007
0.002
 4
3
3
4
4
1
1
1
1
1
  S
Al2O3
MgO
TiO2
Na2O
  %
%
%
%
%
      0.392
0.701
0.502
0.058
0.111
      0.005
0.016
0.004
0.001
0.001
 4
4
4
4
3
1
1
1
1
2
  K2O
V2O5
Cr2O3
NiO
CuO
  %
%
%
%
%
      0.705
0.020
0.040
0.012
0.006
      0.003
0.002
0.001
0.001
0.002
 4
3
3
3
3
1
1
1
1
1
  ZnO
PbO
  %
%
      1.19
0.018
    < 0.01
0.001
 4
3
1
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Atomic absorption spectrometry

Comment
Thermal treatment of material before weighing: 600°C, 1 h