"Excellence Laboratory Technische Compliance Level III" by GAZ GmbH (Attestation no. GAZ-TCL-12-02-14-01)

CERTIFIED REFERENCE MATERIAL
SX32-35
BF-slag

Version: 001      Date of certification: 21.08.13      Sample form: Powder < 0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Ca
CaO
SiO2
Fe
Mn
  %
%
%
%
%
     24.55
34.35
39.33
2.87
0.341
      0.14
0.19
0.13
0.03
0.002
 6
6
3
6
7
1
1
1
1
1
  P2O5
S
Al2O3
MgO
TiO2
  %
%
%
%
%
      0.015
1.539
15.68
6.289
0.229
      0.001
0.038
0.06
0.020
0.007
 3
5
6
7
4
1
1,2
1
1
1
  Na2O
K2O
SrO
BaO
ZrO2
  %
%
%
%
%
      0.103
0.090
0.072
0.107
0.064
      0.006
0.002
0.002
0.002
0.004
 3
4
4
3
4
3
1
1
1
1
  V2O5
Cr2O3
  %
%
      0.004
0.005
      0.001
-.-
 2
1
1
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection
3: Atomic absorption spectrometry
 

Comment
Thermal treatment of material before weighing: 105°C, 1 h