Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX29-01
BF casthouse dust

Version: 003      Date of certification: 27.07.06      Sample form: Powder <0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe
Mn
P2O5
  %
%
%
%
%
      5.28
4.28
59.37
0.367
0.153
      0.02
0.02
0.13
0.007
0.002
 6
6
3
6
6
1
1
1
1
1
  S
Al2O3
MgO
TiO2
Na2O
  %
%
%
%
%
      0.488
0.961
1.147
0.068
0.119
      0.007
0.013
0.014
0.001
0.001
 6
6
6
6
3
1
1
1
1
2
  K2O
V2O5
Cr2O3
NiO
ZnO
  %
%
%
%
%
      0.778
0.020
0.038
0.015
0.267
      0.002
0.002
0.002
0.001
0.001
 6
4
4
4
6
1
1
1
1
1
  PbO
  %
      0.006
      0.001
 3
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Atomic absorption spectrometry

Comment
Thermal treatment of material before weighing: 600°C, 1 h