Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
CaO |
% |
1.609 |
0.004 |
3 |
1 |
SO3 |
% |
0.026 |
0.002 |
3 |
2 |
K2O |
% |
0.089 |
< 0.001 |
4 |
1 |
H2O 900°C |
% |
1.02 |
0.01 |
3 |
5 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
2: Combustion with IR-detection |
3: Atomic absorption spectrometry |
4: Digestion by acids, coulometric detection |
5: Combustion with detection with IR-/ UV-absorption |
  |