Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX57-07
Uncover compound

Version: 002      Date of certification: 27.05.08      Sample form: Powder < 0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe2O3
Mn3O4
P2O5
  %
%
%
%
%
      1.78
82.15
1.50
0.278
0.443
    < 0.01
0.08
0.02
0.001
0.003
 3
3
3
3
3
1
1
1
1
1
  S
Al2O3
MgO
TiO2
Na2O
  %
%
%
%
%
      0.210
0.223
5.086
0.223
0.117
      0.009
0.002
0.075
0.001
0.005
 3
3
3
3
3
2
1
1
1
3
  K2O
C tot.
CO2
H2O 900°C
  %
%
%
%
      1.89
4.03
0.158
1.82
      0.01
0.02
0.007
0.03
 3
3
3
3
1
2
4
5
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection
3: Atomic absorption spectrometry
4: Digestion by acids, coulometric detection
5: detection with IR-/ UV-absorption after combustion