Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX11-35
Iron ore

Version: 001      Date of certification: 12.07.06      Sample form: Powder < 0.100 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe
FeO
Mn
  %
%
%
%
%
      0.011
0.696
64.69
0.06
1.520
      0.001
0.008
0.08
0.01
0.003
 4
4
4
3
4
1
1
1
2
1
  P2O5
S
Al2O3
MgO
TiO2
  %
%
%
%
%
      0.140
0.006
1.49
0.033
0.052
      0.002
0.001
0.01
< 0.001
0.002
 4
3
4
5
4
1
3
1
4
1
  K2O
C tot.
CO2
H2O 900°C
  %
%
%
%
      0.016
0.069
0.007
2.31
      0.001
0.002
0.001
0.10
 4
3
3
3
1
3
5
6
* Measuring method
1: X-ray fluorescence spectrometry
2: Titrimetry
3: Combustion with IR-detection
4: Atomic absorption spectrometry
5: Digestion by acids, coulometric detection
6: Combustion with detection with IR-/ UV-absorption

Comment
Thermal treatment of material before weighing: 105°C, 4 h