Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe tot.
Mn3O4
Al2O3
  %
%
%
%
%
      0.096
27.95
14.51
0.179
11.00
      0.004
0.11
0.07
0.011
0.07
 3
3
3
3
3
1
1
1
1
1
  MgO
TiO2
V2O5
Cr2O3
WO3
  %
%
%
%
%
      7.29
0.486
0.270
33.41
0.019
      0.06
0.006
0.003
0.19
0.002
 3
3
3
3
3
1
1
1
1
1
  NiO
CO2
C tot.
H2O 900°C
  %
%
%
%
      0.090
0.013
0.326
0.129
      0.001
0.003
0.017
0.008
 3
3
3
3
1
2
3
4
* Measuring method
1: X-ray fluorescence spectrometry
2: Digestion by acids, coulometric detection
3: Combustion with IR-detection
4: Detection with IR-/ UV-absorption after Combustion

Comment
Thermal treatment of material before weighing: 105°C, 4 h