CERTIFIED REFERENCE MATERIAL
SX32-39
BF-slag

Version: 001      Date of certification: 20.10.25      Sample form: Powder < 0.0125 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe
Mn
S
  %
%
%
%
%
     42.96
36.54
0.188
0.158
1.065
      0.08
0.04
0.004
0.005
0.008
 5
3
5
5
6
1
1
1
1
1,2,3
  Al2O3
MgO
TiO2
Na2O
K2O
  %
%
%
%
%
     10.85
7.02
0.435
0.232
0.332
      0.03
0.04
0.009
0.006
0.002
 4
4
5
4
5
1
1
1
1
1
  SrO
BaO
Y
ZrO2
  %
%
%
%
      0.069
0.069
0.006
0.037
      0.001
0.001
0.001
0.005
 4
4
4
4
1
1
1
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Gravimetry
3: Combustion with IR-detection