Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX01-03
Ca-aluminate

Version: 001      Date of certification: 13.08.10      Sample form: Powder < 0.125 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  CaO
SiO2
Fe2O3
MnO
Al2O3
  %
%
%
%
%
     23.38
0.450
0.289
0.024
68.8
      0.07
0.010
0.008
0.001
0.2
 4
5
4
5
3
1
1
1
1
1
  MgO
TiO2
K2O
SrO
V2O5
  %
%
%
%
%
      3.53
0.067
0.296
0.009
2.36
      0.01
0.002
0.006
0.002
0.02
 5
6
6
3
5
1
1
1
1
1
  Cr2O3
MoO3
  %
%
      0.028
0.014
      0.006
0.004
 3
3
1
1
* Measuring method
1: X-ray fluorescence spectrometry
 

Comment
Thermal treatment of material before weighing: 900°C, 1 h