Dillinger heavy plates for a dumper at Dillinger plant
In our steel work not only heavy plates are rolled. In the location of Dillingen, Dillinger also produces about 1.5 million t of by-products per year in the crude steel production unit.
Huge excavators - usually used in mines- break the slag after it has been transported from the slag patches of the ironworks and blast furnace. Afterwards the up to 5,000 kg heavy boulders, which can still be up to 250 °C hot are loaded onto dumpers. Impact on the dumper bodies cannot be avoided. The dumper body must stand firm under these rough conditions with 20 load cycles with constant impacts.
Therefore, wear resistant DILLIDUR steels were demanded in the tendering as plates for the dumper body. The application of DILLIDUR among heavy duty conditions in the work of Dillinger allows it, to optimise our DILLIDUR steels constantly on the needs of the customers.
Quality | DILLIDUR 400 V |
---|---|
Wall thickness | 10 - 15 mm |
Head of Sales Department, Machinery & Construction Equipment, Protection
Tel.: +49 6831 472385
Fax: +49 6831 47992681
E-Mail
Head of Marketing & Technical Support, Machinery & Construction Equipment, Steel & Service Center, Plate Processing
Tel.: +49 6831 475658
Fax: +49 6831 47999036
E-Mail
Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.
© 2016 Dillinger All rights reserved.
AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar
Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz
Imprint
| Data privacy statement
| T&C