Heavy skeleton rock bucket made of DILLIDUR
The bucket with a capacity of more than 5 cubic meters and a weight of more than 7 tons is custom made for a 85 tons excavator. Because of the heavy duty work and extreme wear in a limestone quarry the skeleton rock bucket is made of wear resistant DILLIDUR steel.
The side plates and the bars are made out of 60 mm thick DILLIDUR 400 V. For the delta cutting edge the highly crack resistant and very tough DILLIDUR IMPACT in 90 mm thickness is used.
Quality | DILLIDUR 400 V, DILLIDUR IMPACT |
---|---|
Wall thickness | 60 mm (DILLIDUR 400 V), 90 mm (DILLIDUR IMPACT) |
Head of Sales Department, Machinery & Construction Equipment, Protection
Tel.: +49 6831 472385
Fax: +49 6831 47992681
E-Mail
Head of Marketing & Technical Support, Machinery & Construction Equipment, Steel & Service Center, Plate Processing
Tel.: +49 6831 475658
Fax: +49 6831 47999036
E-Mail
Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.
© 2016 Dillinger All rights reserved.
AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar
Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz
Imprint
| Data privacy statement
| T&C