Four butane storage spheres for Morocco were built in 2010 and 2011 with Dillinger plates.
The plant owner is AFRIQUIA GAZ MAROC in Jorf Lasfar. The four spheres each have a diametre of 23770 mm, a volume of 7000 m³ and a dead weight of 530 t. The design pressure is 7.5 bar and the design temperature –20 °C to +50 °C. The spheres were constructed in accordance with the code CODAP 2000. Dillinger delivered 1884 t of heavy plates in steel grade P355GH mod. in thickness up to 30 mm, width up to 3m and length up to 12m. The plates had to fulfill Charpy-requirements at -20 °C.
Opening date | Spring 2011 |
---|---|
Country | Morocco |
Quality | P355GH mod. |
Operator | AFRIQUIA GAZ MAROC |
Pressure | 7.5 bar |
Diameter | 23770 mm |
Case temperature | –20 °C to +50 °C |
Engineer's society | TISSOT Industrie |
Delivered quantity | 1884 t |
Emplacement | Jorf Lasfar |
Wall thickness | up to 30 mm |
Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.
© 2016 Dillinger All rights reserved.
AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar
Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz
Imprint
| Data privacy statement
| T&C