For the solar power station Andasol 1 in Granada (Spain) with an annual capacity of 176 gigawatt hours, Dillinger has supplied 4 heads and 20 shells made of 320t SA302B in thickness up to 90 mm and width up to 4.240 mm.
With these the customer fabricated 4 heat exchangers each with a length of 22 m and an outer diameter of 1,985 mm.
Opening date | 2009 |
---|---|
Country | Spain |
Quality | SA302B |
Building owner | Solar Millenium AG |
Delivered quantity | 4 heads aand 20 shells - 320 t |
Wall thickness | up to 90 mm |