DILLIDUR now fulfills the highest customer requirements even in a record plate thickness of 200 mm!
A special application challenged the Dillinger development team: the high wear resistance of a DILLIDUR 400 should be reached into the core of an extremely thick 200 mm plate.
Therefore, Dillinger developed a tailor made variation of DILLIDUR 400. Of course, this quality should be also reliably suitable for thermal cutting and welding even in this extreme plate thickness.
The reliable processing was proven directly in a first order at our subsidiary Ancofer Stahlhandel GmbH. Various flame-cut parts were easily cut with Dillinger’s information and are already on the way to the end customer.
With our wear resistant DILLIDUR-grades we manage again to combine the properties which are so important for our customers: ultra-high wear resistance plus reliable processability, even in a record plate thickness of 200 mm.
Head of Sales Department, Steel & Service Center, Plate Processing
Tel.: +49 6831 472195
Fax: +49 6831 474580
E-Mail
Head of Marketing & Technical Support, Machinery & Construction Equipment, Steel & Service Center, Plate Processing
Tel.: +49 6831 475658
Fax: +49 6831 47999036
E-Mail
Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.
© 2016 Dillinger All rights reserved.
AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar
Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz
Imprint
| Data privacy statement
| T&C