05. November 2019
Dillinger and its Chinese partner BMM presented from October 25th to 28th DILLIDUR special steels for coal mining applications and customized wear parts.
BMM is the distributor for DILLIDUR special steel plates from stock in China. BMM has over 2 decades of experience in fabricating complex parts made of DILLIDUR.
In underground coal mining DILLIDUR 450 is used for example in armored face conveyors. Here a good balance between the hardness over the plate thickness and a reliable workability are essential.
In roof supports the high strength DILLIMAX steels are widely used. In some tension loaded parts the very high strength DILLIMAX 965B in plate thickness up to 180 mm takes the enormous tension loads.
General Manager Marketing & Technical Support
Tel.: +49 6831 474708
Fax: +49 6831 473089
E-Mail
Sales Earth moving & Mining equipment, Mold & Die construction, Protection applications
Tel.: +49 6831 472223
Fax: +49 6831 47992472
E-Mail
Sales Heavy Machinery, Stockists & Steel Service Centers
Tel.: +49 6831 472195
Fax: +49 6831 474580
E-Mail
Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.
© 2016 Dillinger All rights reserved.
AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar
Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz
Imprint
| Data privacy statement
| T&C