Since its introduction beginning 2016, DILLIDUR 550 completes our product portfolio of DILLIDUR brand steels with the highest hardness of 550 Brinell.
DILLIDUR 550 is available in plate thicknesses from 10 to 51 mm and plate widths up to 3,300 mm. Even higher thicknesses are possible on request. DILLIDUR 550 is used when highest wear resistance is required, for example in earthmoving machines and recycling machines as shredders.