Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
CaO |
% |
11.60 |
0.02 |
7 |
1 |
SO3 |
% |
0.091 |
0.002 |
6 |
1,2 |
K2O |
% |
3.29 |
0.01 |
7 |
1 |
Co3O4 |
% |
0.007 |
0.001 |
4 |
1 |
CO2 |
% |
0.045 |
0.007 |
3 |
4 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
2: Combustion with IR-detection |
3: Atomic absorption spectrometry |
4: Digestion by acids, coulometric detection |
5: detection with IR-/ UV-absorption after Combustion |
  |
Comment |
Thermal treatment of material before weighing: 105°C, 1 h |