Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
Ca |
% |
46.48 |
0.07 |
3 |
1 |
S |
% |
1.18 |
0.02 |
4 |
1 |
K2O |
% |
0.495 |
0.003 |
4 |
1 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
2: Atomic absorption spectrometry |
Comment |
Thermal treatment of material before weighing: 800°C, 1 h |