CERTIFIED REFERENCE MATERIAL
SX02-11
Cement

Version: 002      Date of certification: 09.10.07      Sample form: Powder < 0.100 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Ca
SiO2
Fe2O3
Mn3O4
P2O5
  %
%
%
%
%
     40.63
25.04
2.98
0.172
0.137
      0.06
0.16
0.01
0.002
0.002
 6
4
5
6
4
1
1
1
1
1
  S
Al2O3
MgO
TiO2
Na2O
  %
%
%
%
%
      1.48
6.86
2.79
0.319
0.156
      0.04
0.03
0.01
0.004
0.004
 5
6
6
6
3
1
1
1
1
2
  K2O
SrO
BaO
V2O5
  %
%
%
%
      0.524
0.083
0.041
0.014
      0.002
0.001
0.002
0.001
 4
3
4
3
1
1
1
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Atomic absorption spectrometry

Comment
Thermal treatment of material before weighing: 800°C, 1 h