Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SX02-09
Cement

Version: 002      Date of certification: 09.10.07      Sample form: Powder < 0.100 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Ca
SiO2
Fe2O3
Mn3O4
P2O5
  %
%
%
%
%
     48.78
21.95
0.204
0.025
0.043
      0.05
0.05
0.004
0.001
0.001
 3
3
4
4
4
1
1
1
1
1
  S
Al2O3
MgO
TiO2
Na2O
  %
%
%
%
%
      1.19
4.63
0.717
0.095
0.078
      0.03
0.01
0.005
0.001
0.001
 5
4
4
3
3
1
1
1
1
2
  K2O
SrO
BaO
  %
%
%
      1.01
0.051
0.028
    < 0.01
0.001
0.001
 3
3
3
1
1
1
* Measuring method
1: X-ray fluorescence spectrometry
2: Atomic absorption spectrometry

Comment
Thermal treatment of material before weighing: 800°C, 1 h