Laboratory accredited by GAZ, (Association for the Accreditation and Certification GmbH) Attestation no. 91021

CERTIFIED REFERENCE MATERIAL
SL77-01
Mn

Version: 006      Date of certification: 19.08.10      Sample form: Powder 0.200-0.400 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Si
Fe
Mn
P
S
  %
%
%
%
%
      1.09
2.07
95.83
0.056
0.0160
      0.01
0.02
0.05
< 0.001
0.0001
 5
5
5
5
2
1
1
1
1
2
  Al
Cr
Co
Ni
Cu
  %
%
%
%
%
      0.0015
0.403
0.0012
0.0071
0.0069
      0.0003
0.023
< 0.0001
0.0006
0.0001
 5
5
4
6
6
3
1
3
1,3
1,3
  Zn
C
  %
%
      0.0011
0.120
      0.0001
0.003
 5
5
3
4
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection
3: ICP with optical emission spectrometry
4: Combustion with coulometric detection