"Excellence Laboratory Technische Compliance Level III" by GAZ GmbH (Attestation no. GAZ-TCL-12-02-14-01)

CERTIFIED REFERENCE MATERIAL
SL24-09
Fe-Ti

Version: 001      Date of certification: 19.10.17      Sample form: Powder 0.040-0.200 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Si
Fe
Mn
P
Al
  %
%
%
%
%
      0.180
19.27
0.192
0.004
2.93
      0.010
0.07
0.002
0.001
0.01
 3
4
3
3
3
1
1
1
1
1
  Mg
Ti
Zr
V
Nb
  %
%
%
%
%
      0.070
72.74
0.383
1.167
0.072
      0.004
0.11
0.005
0.012
0.005
 3
3
4
4
4
1
1
1
1
1
  Cr
Mo
Ni
Cu
Sn
  %
%
%
%
%
      0.384
0.814
0.047
0.074
0.246
      0.005
0.007
0.002
0.004
0.008
 3
4
3
3
4
1
1
1
1
1
* Measuring method
1: X-ray fluorescence spectrometry