"Excellence Laboratory Technische Compliance Level III" by GAZ GmbH (Attestation no. GAZ-TCL-12-02-14-01)

CERTIFIED REFERENCE MATERIAL
SL17-04
Fe-B

Version: 001      Date of certification: 19.10.17      Sample form: Powder 0.125-0.200 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Si
Fe
Mn
P
Al
  %
%
%
%
%
      0.229
79.94
0.299
0.015
0.064
      0.008
0.16
0.002
0.001
0.004
 4
4
4
3
3
1
1
1
1
1
  Ti
Cr
W
Ni
Cu
  %
%
%
%
%
      0.011
0.038
0.015
0.012
0.013
      0.001
0.005
0.002
0.001
0.002
 4
3
3
4
3
1
1
1
1
1
  B
C
  %
%
     19.13
0.322
      0.21
0.016
 4
3
2
3
* Measuring method
1: X-ray fluorescence spectrometry
2: ICP with optical emission spectrometry
3: Combustion with IR-detection