"Excellence Laboratory Technische Compliance Level III" by GAZ GmbH (Attestation no. GAZ-TCL-12-02-14-01)

CERTIFIED REFERENCE MATERIAL
SL16-03
Fe-Cr Carburé

Version: 002      Date of certification: 21.12.15      Sample form: Powder 0.100-0.200 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Si
Fe
Mn
P
S
  %
%
%
%
%
      0.216
24.03
0.115
0.024
0.059
      0.010
0.23
0.004
0.001
0.010
 4
4
5
5
3
1
1
1
1
2
  Al
Mg
Ti
V
Cr
  %
%
%
%
%
      0.011
0.019
0.010
0.095
67.21
      0.002
0.003
0.002
0.001
0.14
 4
4
5
4
4
1
1
1
1
1
  Co
Ni
C
  %
%
%
      0.055
0.509
7.49
      0.001
0.008
0.12
 5
3
3
1
1
2
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection