"Excellence Laboratory Technische Compliance Level III" by GAZ GmbH (Attestation no. GAZ-TCL-12-02-14-01)

CERTIFIED REFERENCE MATERIAL
SL16-02
Fe-Cr Carburé

Version: 002      Date of certification: 09.10.13      Sample form: Powder < 0.100 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Si
Fe
Mn
P
Al
  %
%
%
%
%
      0.153
19.38
0.103
0.014
0.017
      0.007
0.03
0.009
0.001
0.003
 4
4
4
3
4
1
1
1
1
1
  Mg
Ti
V
Nb
Cr
  %
%
%
%
%
      0.049
0.009
0.102
0.006
71.20
      0.006
0.001
0.001
0.001
0.12
 4
4
4
4
3
1
1
1
1
1
  W
Ni
C
  %
%
%
      0.038
0.304
8.12
      0.002
0.008
0.09
 4
4
3
1
1
2
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection