Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
Si |
% |
0.052 |
0.011 |
3 |
1 |
Cr |
% |
0.009 |
0.001 |
3 |
1 |
Pb |
% |
1.31 |
0.05 |
3 |
1 |
* Measuring method | |
1: X-ray fluorescence spectrometry |
  |