CERTIFIED REFERENCE MATERIAL
SL02-02
Cu alloys

Version: 003      Date of certification: 09.06.08      Sample form: Milling 0.200-0.630 mm

Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Fe
Mn
S
Ni
Cu
  %
%
%
%
%
      0.911
0.007
0.037
0.034
98.15
      0.026
0.001
0.004
0.002
0.06
 3
3
3
3
3
1
1
1
1
1
  Zn
Sn
Pb
As
Sb
  %
%
%
%
%
      0.229
0.381
0.139
0.032
0.008
      0.002
0.038
0.005
0.001
0.002
 3
3
3
3
3
1
1
1
1
1
* Measuring method
1: X-ray fluorescence spectrometry