Laboratory
"Excellence Laboratory Technische Compliance Level III" by GAZ GmbH (Attestation no. GAZ-TCL-12-02-14-01)

CERTIFIED REFERENCE MATERIAL
SL01-06
Si-Mn Affiné

Version: 005      Date of certification: 06.04.20      Sample form: Powder 0.090-0.315 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  Si
Fe
Mn
P
S
  %
%
%
%
%
     18.38
14.60
65.24
0.080
0.010
      0.06
0.06
0.11
0.002
0.001
 3
4
3
4
3
1
1
1
1
2
  Ti
V
Cr
Co
Ni
  %
%
%
%
%
      0.121
0.015
0.011
0.013
0.042
      0.003
< 0.001
0.001
< 0.001
0.002
 4
6
5
6
4
1
1,3
1,3
1,3
1,3
  Cu
C
  %
%
      0.017
1.21
      0.001
0.02
 5
3
1,3
2
* Measuring method
1: X-ray fluorescence spectrometry
2: Combustion with IR-detection
3: ICP with high resolution mass spectrometry