| Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
C |
% |
0.0048 |
0.0002 |
12 |
1 |
Cr |
% |
0.0405 |
0.0001 |
12 |
2 |
Co |
% |
11.46 |
0.01 |
12 |
2 |
Ti |
% |
1.28 |
< 0.01 |
12 |
2 |
| * Measuring method | |
| 1: Combustion with coulometric detection |
2: Atomic absorption spectrometry |
| 3: Photometry |
4: Combustion with IR-detection |