Laboratory
"Excellence Laboratory Technische Compliance Level III" by GAZ GmbH (Attestation no. GAZ-TCL-12-02-14-01)

CERTIFIED REFERENCE MATERIAL
SE23-221
alloyed steel

Version: 005      Date of certification: 18.08.21      Sample form:  
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  C
S
N
  %
%
%
      0.0622
0.0007
0.0031
      0.0003
0.0001
0.0001
 3
3
3
1
2
3
* Measuring method
1: Combustion with coulometric detection
2: Combustion with IR-detection
3: Hot extraction with HC and IR detection