| Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
C |
% |
0.0438 |
0.0003 |
5 |
1 |
Cr |
% |
0.0290 |
0.0001 |
5 |
2 |
As |
% |
0.0029 |
0.0002 |
4 |
3 |
Pb |
% |
0.00004 |
0.00001 |
5 |
2 |
Ca |
% |
0.0016 |
< 0.0001 |
5 |
2 |
| * Measuring method | |
| 1: Combustion with IR-detection |
2: Atomic absorption spectrometry |
| 3: Photometry |
  |