| Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
C |
% |
0.1658 |
0.0004 |
21 |
1 |
Cr |
% |
0.0128 |
0.0003 |
10 |
2 |
Co |
% |
0.0046 |
0.0001 |
10 |
2 |
Ti |
% |
0.0008 |
< 0.0001 |
10 |
2 |
| * Measuring method | |
| 1: Combustion with coulometric detection |
2: ICP with optical emission spectrometry |
| 3: Combustion with IR-detection |
4: ICP with quadrupol mass spectrometry |