| Analyte | Unit | Certified value | Confidence interval (95%) |
No. of independent repeated series |
Measuring method* |
C |
% |
0.0362 |
0.0002 |
5 |
1 |
Cr |
% |
0.0075 |
< 0.0001 |
5 |
2 |
Co |
% |
0.0048 |
< 0.0001 |
5 |
2 |
Ca |
% |
0.0001 |
< 0.0001 |
5 |
2 |
| * Measuring method | |
| 1: Combustion with coulometric detection |
2: Atomic absorption spectrometry |
| 3: Photometry |
4: Combustion with IR-detection |