Laboratorium
Postfach 1580, 66748 Dillingen
CERTIFIED REFERENCE MATERIAL
SE21-351
unalloyed steel

Version: 001      Date of certification: 28.04.25      Sample form: 0,200 - 400 mm
Analyte Unit Certified value Confidence
interval (95%)
No. of independent
repeated series
Measuring
method*
  C
S
N
  %
%
%
      0.0510
0.0077
0.0017
      0.0006
0.0001
0.0002
 4
3
3
1
2
3
* Measuring method
1: Combustion with coulometric detection
2: Combustion with IR-detection
3: Hot extraction with HC and IR detection